LR Grade DH62 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade EH50 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade FH50 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade AH50 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade DH50 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade EH46 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade FH46 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.18 0.55 1.60 0.020 0.020 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade AH46 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade DH46 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade EH42 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade FH42 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.18 0.55 1.60 0.020 0.020 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade AH42 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
LR Grade DH42 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
DNV Grade E690 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
DNV Grade F690 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.18 0.55 1.60 0.020 0.020 0.020 Yield Strength (MPa) min. ...
china
Member
DNV Grade A690 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
DNV Grade D690 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
DNV Grade E620 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
DNV Grade F620 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.18 0.55 1.60 0.020 0.020 0.020 Yield Strength (MPa) min. ...
china
Member
DNV Grade A620 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china