Home Products

abs shipbuilding steel plate

Refine Search

Related Products

Results forabs shipbuilding steel platefrom 132358 Products.
KR Grade E63 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade F63 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.18 0.55 1.60 0.020 0.020 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade A63 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade D63 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade E56 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade F56 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.18 0.55 1.60 0.020 0.020 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade A56 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade D56 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade E51 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade F51 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.18 0.55 1.60 0.020 0.020 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade A51 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade D51 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade E47 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade F47 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.18 0.55 1.60 0.020 0.020 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade A47 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.21 0.55 1.70 0.030 0.030 0.020 Yield Strength (MPa) min. ...
china
Member
KR Grade D47 Shipbuilding Steel Plate Chemical Composition and Mechanical Property C max Si max Mn P max S max N max. 0.20 0.55 1.70 0.025 0.025 0.020 Yield Strength (MPa) min. ...
china
Member
ASTM A131 Grade D Shipbuilding Steel Plate Chemical Composition and Mechanical Property Grade C % Si % Mn.Min % P % S % C+Mn/6 ASTMA131 D 0.21 0.10-0.35 0.60 0.035 0.035 0.40 Grade ...
china
Member
ASTM A131 Grade E Shipbuilding Steel Plate Chemical Composition and Mechanical Property Grade C % Si % Mn .Min% P % S % C+Mn/6 ASTMA131 E 0.18 0.10-0.35 0.70 0.035 0.035 0.40 Grade ...
china
Member
ASTM A131 Grade A Shipbuilding Steel Plate Chemical Composition and Mechanical Property Grade C % Si % Mn %Min P % S % C+Mn/6 ASTMA131 A 0.21 0.50 2.5xC 0.035 0.035 0.40 Grade ...
china
Member
ASTM A131 Grade B Shipbuilding Steel Plate Chemical Composition and Mechanical Property Grade C % Si % Mn Min % P % S % C+Mn/6 ASTM A131 B 0.21 0.35 0.60 0.035 0.035 0.40 Grade ...
china
Member
Page 13 of 50 |< << 9 10 11 12 13 14 15 16 17 >> >|