ASME SB 167 Nickel Chromium Cobalt Alloy UNS N07090 Nimonic90 / W. Nr.2.4632
Nimonic90 / UNS N07090 / W. Nr.2.4632 alloy seamless pipe customization
Nimonic 90*(UNS N07090/W. Nr.2.4632)
Introduction NIMONIC 90 (UNS N07090/W. Nr. 2.4632) is a wrought nickel-chromium-cobalt base alloy strengthened by additions of titanium and aluminum. It has been developed as an age-hardenable creep resisting alloy for service at temperatures up to 920°C | ||||||||||||||||
| ||||||||||||||||
Application The alloy is used for turbine blades, discs, forgings, ring sections and hot-working tools. Also used to make Aerospace fasteners. | ||||||||||||||||
Equal grades
| ||||||||||||||||
Chemical composition
| ||||||||||||||||
Standard AMS 5829 | ||||||||||||||||
Forms of product available Plate, sheet, strip, bar, wire, rod, pipe, tube, forging. | ||||||||||||||||