Home Companies Hubei Nuojin Sen Technology Co.,Ltd

Base Mix Ratio Solder Resist Mask , Blue Color Photosenstive / Photo Curing Liquid Ink

Hubei Nuojin Sen Technology Co.,Ltd
Active Member

Contact Us

[China] country

Address: 29th floor room 15 No.5 Commercial building B block ,the 2nd section Wuchang Fu west,No.32 Wenzhi street,Hongshan district,Wuhan city,China

Contact name:

Inquir Now

Hubei Nuojin Sen Technology Co.,Ltd

Base Mix Ratio Solder Resist Mask , Blue Color Photosenstive / Photo Curing Liquid Ink

Country/Region china
City & Province wuhan hubei
Categories Newsprint Paper
InquireNow

Product Details

Blue color photosenstive and photo curing liquid ink for pcb industry

 

ItemsTechnical featuresNotes
ColorBlue 
Viscosity (25℃)10±2dPa﹒sVT-04F
Fineness≤5µm0 ~25µm Fineness gauge
Solid content50±5% 
Density (25℃)1.10 ~1.20 g/ml 
Resolution50µm (2.0mil) 
Adhesion100/100Laceration experiment
Plating resistanceCopper ,Tin ,Nickle and AurumNormal plating technics
Hardness≥2HPencil harder
EtchingAcidic/Alkaline etching solution 
Pre-baking limit75℃, 60min 
Package5.0kg/bucket , 20kg/boxAccording to customer requirements
Shelf time6 months since the date of manufactureStore below 25℃ in dark

 

Working procedure

1. Mixing

Mixing a small amount main agent with hardener and stirring thoroughly,then mixing the mixture above with the remanent main agent,add appropriate diluent and stirring 5-10 minutes. The viscosity of ink is adjusted to 120 PS if printed by hand. And it is adjusted to 180 PS if printed by machine.It is adjusted to 200 PS if it is aluminum tamponade .The viscosity of ink mixed above is measured at 25 degrees. Please use the special diluent of our company if the viscosity of ink needs to adjust.

  • Remain time

10-15 minutes after stiring uniformly

  • Ordinary boards:43T;Chemical-plating Aurum or Tin boards:36T
  • Pre-baking

1) Single side printing separately

First side:72-76 degrees,15-18 min

Second side:72-76 degrees,30-35 min

  • Double sides printing simultaneously:72-76 degrees,40-60min
  • Exposure

300-500mJ/cm2,Black ink:600-750mJ/cm2,exposure step:10-12 steps

  • Developing:

Developing solution:0.8-1.2wt% Na2CO3 or K2CO3 aqueous solution

Developing solution temperature:28-32 degrees

Spray pressure:1.5-2.5kg/cm2

Developing time:40-90 seconds

  • Post cure

Spray Tin board:150 degrees*(60-120min)

Chemical-plating Aurum board:150 degrees*(50-60min)

Thick copper plate,boards printed with black ink should be post-black in subsection:75 degrees*(60-120min)+100 degrees*30 min+150 degrees*(60-90min)

  • Safe time

6 months since the date of manufacture,store below 25 degree in dark

  • Attention:

1) Mixing the ink fully before using

2) We will offer you special diluent or PMA if the ink need dilute

3) The values above are based on experiments in our lab.Experiments need to be carried out in order to get proper using condition.

Hot Products

Screen / Roll Printing UV Curable Solder Mask PCB Ink 20kg / Box Package Items Technical features ...
Screen / Roll Printing White Solder Mask , UV Curable Solder Mask PCB Ink Items Technical features ...
Liquid photoimage,blue color etching resist plating and etching line ink Items Technical features ...
Glass etching resist ink,black color,liquid photo image curing for industry Items Technical features ...
Blue color photosenstive and photo curing liquid ink for pcb industry Items Technical features Notes ...
Beige led and pcb ink ,liquid and photo image solder resist mask Items Technical features Notes ...