Chongqing Aorun Industrial Co., Ltd. |
|
Quick Detail:
Name | Epoxy Resin 3248 | Usage | Woodworking |
Mixing Ratio | A: B = 2:1 (By weight) | Curing time | About 10-12 hrs at room temperature |
Description:
Our Epoxy resin can be cured under normal temperature, two components system hard resin, natural defoaming, yellow resistance, high transparency, bright in surface, it can be also cured at high temperature for faster curing.
With our Epoxy Floor Coatingsystem, you get a whole range of
additional Advantages including:
• Industrial Strength Epoxy
• Waterproof Barrier, Against Moisture, Corrosion Inhibiting,
Excellent Adhesion
• Designed for commercial, industrial, and residential concrete,
cement, wood and tile Floor coating
• Warm, comfortable feel underfoot.
• Non-slip finish.
• Colour stability.
• Abrasion resistant.
• Seamless.
• Glossy, satin or mat surface.
• Light and weather resistant.
• High UV stability under normal daylight conditions.
• Reduced noise transfer providing quieter floors, reduces
horizontal noise transmission.
• Hygienic floor finish, low dust retention, easy to clean,
resilient surface.
• Light reflecting aesthetic floor finish.
• Available in over 150 RAL colors.
Items | Units/conditions | Technical Data |
Viscosity | Shore-D | 80-85 |
Volume resistivity | 25℃/ Ω./ cm | 4.3x1015 |
Surface resistivity | 25℃/ Ω. | 2.6x1014 |
Dielectric strength | 25℃ KV/MM | 25 |
Coefficient of linear expansion | CM/K | <6.1x10-5 |
Glass transition temperature | ℃ | >90 |
Temperature resistant | ℃ | -60~120 |
Notice:
1,The operating environment should be ventilative and should keep
away from fire. Closely sealed after use.
2, Avoid eye contact, in case of contact, wash with plenty of water
and get medical attention immediately.
3, If contact skin, wrap with clean cloth or paper, and wash it
with water and soap.
4, Keep away from children.
5, Please take a trial before application to avoid usage mistake.
FAQ:
Q1. Will the Table Epoxy Resin turn yellow over time?
A: No, because we add HALS, which is UV protection, it won't change
yellow.
Q2. Does this Table Epoxy Resin tend to scratch over time?
A: Our product is Scratch Resistance, Heat Resistance, Electrical
resistance.
Q3. What is the ideal temperature to make mixtures?
A: The optimal temperature is 25 degrees celsius, because our
laboratory temperature is 25 degrees celsius, but a little hotter
or colder is also ok.
Q4. How long can last if it is not mixed?
A: The shelf life is about 12 months, if you keep it well.