Automatic Electrode Welding Making Manufactruing Battery Assembly Machine I.Introduction This equipment is a special production equipment for making cylindrical battery electrode. ...
|
|
|
Pure tungsten electrodes (AWS classification EWP) contain 99.50% tungsten, have the highest consumption rate of all electrodes and are typically less expensive than “alloyed” counterparts. These electrodes form a clean, ...
|
|
|
|
Great Deals on 6 Electrodes Welding Supplies with 380V Voltage *, *::before, *::after {box-sizing: border-box;}* {margin: 0;}html, body {height: 100%;}body {line-height: 1.5;...
|
|
|
|
W/Cu 90/10 85/15 80/20 75/25 70/30 60/40 Copper Tungsten Electrodes Quick details : Grade: WCu10 WCu15 WCu20 WCu25 WCu30 WCu50 Shape: rod/bar Copper Content: 7%-50% Density: 11.85g...
china
|
|
|
|
#detail_decorate_root .magic-0{border-bottom-style:solid;border-bottom-color:#53647a;font-family:Roboto;font-size:24px;color:#53647a;font-style:normal;border-bottom-width:2px...
|
|
|
|
Grinding / Blank Tungsten Carbide Welding Rod with submicron Description: 1. Material: 100%virgin raw material with submicron and average grain size. Various grades for choice; 2. ...
|
|
|
|
KCF Guide pin , Lower Electrode , Lower Electrode Holder For Lower Electrode Welding KCF is a special metal materials,the main metal elements include iron,chromium,lead,mercury,PBB...
|
|
|
|
Power: 220V AC 50~60HZ Option:110V AC 50~60HZ Total Power: 580W Wire Length: 2 Meters No Load Speed: 30000r/min Temperature: No load 10 min Air Temperature +20ºC Noise(No-load): 90 ...
|
|
|
Pure tungsten electrodes (AWS classification EWP) contain 99.50% tungsten, have the highest consumption rate of all electrodes and are typically less expensive than “alloyed” counterparts. These electrodes form a clean, ...
|
|
|
1% lanthanated tungsten electrodes (AWS classification EWLa-1) contain a minimum of 97.80% tungsten and 0.80 to 1.20% lanthanum, or lanthana. These electrodes have excellent arc starting, low-burn-off rate, good arc ...
|
|
|
1.5% lanthanated tungsten electrodes (AWS classification EWLa-1.5) contain a minimum of 97.80% tungsten and 1.30 to 1.70% lanthanum, or lanthana. These electrodes have excellent arc starting, low-burn-off rate, good arc ...
|
|
|
2% lanthanated tungsten electrodes (AWS classification EWLa-2) contain a minimum of 97.80% tungsten and 1.80 to 2.20% lanthanum, or lanthana. These electrodes have excellent arc starting, low-burn-off rate, good arc ...
|
|
|
2% lanthanated tungsten electrodes (AWS classification EWLa-2) contain a minimum of 97.80% tungsten and 1.80 to 2.20% lanthanum, or lanthana. These electrodes have excellent arc starting, low-burn-off rate, good arc ...
|
|
|
Zirconiated tungsten electrodes (AWS classification EWZr-1) contain a minimum of 99.10% tungsten and .15 to .40% zirconium. A Zirconiated tungsten electrode produces an extremely stable arc and resists tungsten spitting. ...
|
|
|
Zirconiated tungsten electrodes (AWS classification EWZr-1) contain a minimum of 99.10% tungsten and .15 to .40% zirconium. A Zirconiated tungsten electrode produces an extremely stable arc and resists tungsten spitting. ...
|
|
|
2% thoriated tungsten electrodes (AWS classification EWTh-2) contain a minimum of 97.30% tungsten and 1.70 to 2.20% thorium. They are the most commonly used electrodes today and are preferred for their longevity and ease ...
|
|
|
2% thoriated tungsten electrodes (AWS classification EWTh-2) contain a minimum of 97.30% tungsten and 1.70 to 2.20% thorium. They are the most commonly used electrodes today and are preferred for their longevity and ease ...
|
|
|
Pure tungsten electrodes (AWS classification EWP) contain 99.50% tungsten, have the highest consumption rate of all electrodes and are typically less expensive than “alloyed” counterparts. These electrodes form a clean, ...
|
|
|
Zirconiated tungsten electrodes (AWS classification EWZr-1) contain a minimum of 99.10% tungsten and .15 to .40% zirconium. A Zirconiated tungsten electrode produces an extremely stable arc and resists tungsten spitting. ...
|
|
|
2% ceriated tungsten electrodes (AWS classification EWCe-2) contain a minimum of 97.30% tungsten and 1.80 to 2.20% cerium. These electrodes perform best in DC welding at low current settings but can be used proficiently ...
|
|
|