ABS RX710 Datasheet:
Properties | Method | Unit | RX710 |
Physical | |||
Specific Gravity , 23℃ | ASTM D792 | 1.04 | |
Mold Shrinkage , 23℃, 3.2mm , 23℃ | ISO 294-4 | % | 0.4 ~ 0.7 |
Melt Flow Rate , 220℃, 10kg | ASTM D1238 | g/10min | 37 |
Mechanical | |||
Tensile Strength at Yield , 23℃, 50mm/min, 3.2mm | ASTM D638 | Mpa | 40 |
Tensile Elongation at Yield , 23℃, 50mm/min, 3.2mm | ASTM D638 | %, (Min) | 5 |
Tensile Elongation at Break , 23℃, 50mm/min, 3.2mm | ASTM D638 | %, (Min) | 15 |
Tensile Modulus , 23℃, 50mm/min, 3.2mm | ASTM D638 | MPa | 1950 |
Flexural Strength , 23℃, 15mm/min, 3.2mm | ASTM D790 | Mpa | 64 |
Flexural Modulus , 23℃, 15mm/min, 3.2mm | ASTM D790 | MPa | 2150 |
Izod Impact Strength , Notched, 3.2mm, 23℃ | ASTM D256 | J/m | 540 |
Izod Impact Strength , Notched, 3.2mm, -30℃ | ASTM D256 | J/m | 250 |
Izod Impact Strength , Notched, 6.4mm, 23℃ | ASTM D256 | J/m | 470 |
Izod Impact Strength , Notched, 6.4mm, -30℃ | ASTM D256 | J/m | 215 |
Rockwell Hardness , R-Scale | ASTM D785 | 97 | |
Thermal | |||
HDT , Edgewise, 1.82MPa, 6.4mm, Unannealed | ASTM D648 | ℃ | 84 |
VICAT , 50N, 50℃/h | ASTM D1525 | ℃ | 91 |
RTI Electrical | UL 746B | ℃ | 60 |
RTI Mechanical with Impact | UL 746B | ℃ | 60 |
RTI Mechanical without Impact | UL 746B | ℃ | 60 |
Flammability, 1.5mm | UL 94 | HB | |
Flammability, 3.0mm | UL 94 | HB |
ABS RX710 Caution:
1.THIS BAG SHOULD NOT BE USED FOR ANY OTHER PURPOSES EXCEPT FOR PACKING THE PELLETS.
2. SOME PHISICAL AND/OR CHEMICAL PROPERTIES OF THIS PRODUCT MAY CHANGE WHEN IT'S MIXED WITH OTHER CHEMICAL PRODUCTS. PLEASE TEST IT AND CONFIRM BEFORE USING IT IN THE CONDITION ABOVE.
3.KEEP AWAY FROM THE HEAT, SPARK, AND FLAME.
4.DO NOT INHALE GASEMITTED FROM THE HEATED RESIN.