Home Companies Eternal Bliss Alloy Casting & Forging Co.,LTD.

ASTM A297 HP Cobalt Alloy Castings / Investment Casting Heat Resistant Parts

Eternal Bliss Alloy Casting & Forging Co.,LTD.
Active Member

Contact Us

[China] country

Address: 1099 Xinhua Road,214104, Xishan District, Wuxi, Jiangsu,China

Contact name:Juliet Zhu

Inquir Now

Eternal Bliss Alloy Casting & Forging Co.,LTD.

ASTM A297 HP Cobalt Alloy Castings / Investment Casting Heat Resistant Parts

Country/Region china
City & Province wuxi jiangsu
InquireNow

Product Details

High Temperature ASTM A297 HP Investment Cast Heat Resistence Parts EB3381

We produce High Temperature Superalloy Castings Parts with centrifugal cast process, investment process and resin sand cast process.

 

Cobalt base alloys have been used extensively in the past for high temperature applications and have been found to be generally satisfactory except that in some instances they have been lacking in oxidation resistance, when compared to nickel base alloys. However, at high temperatures, on the order of 1800 to 2100 F. nickel base alloys have limited mechanical properties. Accordingly, it would represent an advance in the art if cobalt base alloys could be provided with oxidation resistance comparable to or better than that of nickel base alloys at high temperatures, while retaining the characteristic strength and mechanical properties of cobalt base alloys at high temperatures.

 

Table 1 : Standard Cobalt cobalt alloy Alloy 

 CoCrCWMoNiSiBFeMnOthers
cobalt alloy 1BAL332.4513-2.5*1-2.5*1-
cobalt alloy 3BAL312.513-2.5*1-2.5*1-
cobalt alloy 4BAL31.5114-2.0*1-2.0*1-
BAL281.25-3.0*1-2.5*1-
cobalt alloy 12BAL291.859-2.5*1-2.5*1-
cobalt alloy 20BAL332.4517.5-2.5*1-2.5*1-
cobalt alloy 21BAL270.25-5.52.5*1-3.0*1-
cobalt alloy 31BAL260.57.5-10.51-2.0*1-
cobalt alloy 190BAL263.314-1.01-8.00.5-
cobalt alloy 238BAL260.1-3-1-20.01-
cobalt alloy 306BAL250.42-6.01-4.0*1Nb=5
94BAL28119-5.01-2.5*1V=1
cobalt alloy FBAL25.51.7512.25-22.51-1.5*--
cobalt alloy SF1BAL191.313-1332.53*0.5Cu=0.5
cobalt alloy SF6BAL190.77-132.51.73*0.5Cu=0.5
cobalt alloy SF12BAL1919-13323*0.5Cu=0.5
cobalt alloy SF20BAL191.515-13332*0.5Cu=0.5
TRIBALOY T400BAL80.1*-283*2.4-3*--
TRIBALOY T800BAL170.1*-283*3.2-3*--
DELORO 15--0.06*--BAL2.01.051.5*20Cu=20
DELORO 22-0.700.10--BAL2.31.75---
DELORO 40-7.00.10--BAL3.52.25---
DELORO 50-10.250.45--BAL4.01.854.0--
DELORO 60-14.250.6--BAL2.03.54.0--
DELORO 625-220.1-9BAL--5--
NISTELLE C-16.50.12*4.517BAL0.7-6.0--
TRIBALOY T700-150.10*-32BAL3.25-   
 Hastelloy C22®(UNS N06022)(Max.)
 CMNPSSiCrNiMoCOFeWV
 0.0150.50.020.020.0820.0-22.5Bal.12.5-14.52.52.0-6.02.5-3.50.35
 Hastelloy C276®(UNS N10276)(Max.)
 CMNPSSiCrNiMoCOFeWV
 0.0110.040.030.0814.5-16.5Bal.15.0-17.02.54.0-7.03.0-4.50.35
 Hastelloyx®(UNS N06002)(Max.)
 CMNPSSiCrNiMoCOFeWother
 0.05-0.1510.040.03120.5-23.0Bal.8.0-10.00.5-2.517.0-20.00.2-1.0/
 Monel 400®(UNS NO4400) (Max.) 
 CMNSSiNiCuFe
 0.320.0240.563 min28-342.5
 Monel M400®(UNS NO4400)(Max.)
 CMNSSiNiCuFe
 0.320.0240.563-7028-342.5
 Monel R405®(UNS NO4405)(Max.)
 CMNSSiNiCuFe
 0.320.025-0.060.563.0min28-342.5
 Monel K500®(UNS NO5500)(Max.) 
 CMNSSiNiCuTiAIFe
 0.120.010.563min27-330.862.3-3.152
 Inconel 600(UNS NO6600)(Max.) 
 CMNSSiCrNiCuFe 
 0.1510.0150.514-1772 min0.56.0-10.0
 Inconel 601(UNS NO6601)(Max.)
 CMNSiCrNiCOAIFe
 0.050.30.222.561.5min51.414.1
 Inconel 718(UNS NO7718)(Max.)
 CrNiMoCOCb+TaTiAIFe
 1952.5min3.0555.130.90.518.5
 Chemical Analysis of Incoloy 800® uns(N08800) 
 CCrNiTiAIFeGrain
 0.1 max19.0-23.030.0-35.00.15-0.60.15-0.639.5min/
 Incoloy800H® UNS(N08810)
 CCrNiTiAIFeGrain
 0.05-0.119.0-23.030.0-35.00.15-0.600.15-0.6039.5min5or coarser
 Incoloy800HT® UNS(N08811)
 CCrNiTiAIFeGrain
 0.06-0.1019.0-23.030.0-35.00.25-0.600.25-0.6039.5min5or coarser

 

Dimensions:as per drawings

 

 

Production Process

Step 1: Getting orders.

 

Step 2: Process design by technical department

 

Step 3: Purchase of raw materials and pattern making &checking

 

Step 4: Inspection of raw materials

 

Step 5: Melting by middle-frequency induction furnaces

 

Step 6: Ladle analysis by Spectrometer

 

Step 7: De-oxidization, slag-removal, tapping

 

Step 8: Pouring

 

Step 9: Openning & fettling

 

Step 10: Surface & dimensional check

 

Step 11: Heat treatment

 

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

 

Step 13: Packing

 

Step 14: Shipping

 

 

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.

 

 

Our Trade Show

 

Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.

 

 

Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

www.ebcastings.com


Eternal Bliss Alloy Casting & Forging Co.,LTD.

Add.: J-Sci-Tech Park, Binhu District,Wuxi,214122, Jiangsu,China

Hot Products

High Temperature UM Co-50 Cobalt Alloy Casted Foundry Squiggle Twigs Heat treatment EB9091 We ...
X-40 Cobalts Alloy Castings Parts Temperature 1300 EB9110 We produce High Temperature Superalloy ...
ASTM A297 HP Investment Cast Heat Resistance cobalt alloy 12 Coating EB3379 We produce High ...
cobalt alloy 21 Coating 3mm Thick ASTM A297 HP Investment Cast Heat Resistence Parts EB3380 We ...
High Temperature ASTM A297 HP Investment Cast Heat Resistence Parts EB3381 We produce High ...
cobalt alloy 1 Coating Customized Investment Forging Parts Heat-Resistance Steel 316L EB3385 We ...