Please input your companyname! |
|
la bicomponent low melt fiber, pla bicomponent low melt fiber
Bicomponent Low Melt Fiber Description
PLA bicomponent is the short fiber form Side By Side", a kind of eye-catching PLA fiber developed by US, As a kind
of new hot junction complex fiber,This fiber is thought high in the
world.
After heat treatment, fiber was joined together, forming a
non-woven mould .
Different non-woven fabrics can be got according to different heat
treatment method.
Such as: THROUGH-AIR → Loose non-woven fabrics
CALENDER
→ Non-woven fabrics with high strength.
Specifications of low melt polyester fiber:
1. Fineness | 1.5D~10D |
2. Cut Length | 5MM~76MM |
3. Material | 100% PLA Fiber |
4. Color | White Color |
5. Melting point | 110°C |
6. Delivery Time | Within 15 days after firm order |
7. Package | PP Woven Bag 280kg/ Pressed Bale 20'GP: 35 Bales |
8. Production Capacity | 45000 Tons Per Year |
9. Sheath/core structure:
Sheath(PDLA): 115°C~ 130 °C 20%
Core(PLLA): 165°C ~ 170 °C 80%
| |
10.Application: - Suitable for filling pillow, toys, quits, cushion etc. -Car Interior, Doortrim etc.
| |
11.Advantage - Excellent thermal bonding. - Easy to mix with other fibers. - Excellent durability, Excellent resilience & Washable. - Stable processibility.
|