Stellite 6 Polystel 6 Hoganas 2537 Hard Facing Rod Red Color Extrusion Screws Flights Tong Bits Product Description WL-Co6 is the most widely used of the wear resistant cobalt...
|
|
|
|
Ultra-Durable Tungsten Carbide Sealing Rings - Maximum Performance & Longevity Description Tungsten Carbide Seal Rings are an ideal choice for sealing applications that require ...
|
|
|
|
Chinese API sucker rod pump Petroleum Equipment API 11AX cobalt base valve balls and seats downhole equipment sucker rod pump barrel tube 1. API-11AX & Non-API Rod, Tubing & ...
|
|
|
|
Zirconia Ceramic Foam Filters Zirconia Ceramic Foam Filters are used for molten all types of steel like unalloyed, low alloyed, stainless and high-alloyed as well as Nickel and ...
|
|
|
|
GH2747 is an iron-nickel-chromium-based precipitation hardening high-temperature alloy. It is used in a solid solution state. Its long-term operating temperature is 1100~1250°C, ...
|
|
|
|
The classification of tungsten steel is carried out according to ISO standards. This classification is based on the material type of the workpiece (eg P, M, K, N, S, H grades). The ...
|
|
|
|
Digital PFM Dental Crown Restoration PFM Restoration Crown Description: PFM restorations can be made from different metals, such as base metal alloys (cobalt, nickel, chromium), ...
china
|
|
|
|
OD24.5mm K50 unground carbide rods for high-speed cutting tools ISO Grade Grain Cobalt Density Hardness T.R.S Application um % g/cm3 HRA N/mm2 K30-K50 0.4 12 14.05 92.6 4200 High...
|
|
|
|
High Strength Nickel Alloy SEAMLESS Pipe , ASME SB167 Inconel Alloy Steel Seamless Pipe Nickel alloys are used for high-temperature and highly corrosive media. Such conditions are ...
|
|
|
|
Stellite 21 Cobalt Base Hardfacing, Welding & Thermal Spraying Powder Product Description WL Co21 is recommended for applications involving cavitation, erosion, corrosion and/or ...
|
|
|
|
Tungsten steel sintering process The classification of tungsten steel is carried out according to ISO standards. This classification is based on the material type of the workpiece. ...
|
|
|
|
High-speed cutting tools with ground carbide rods with chamfer 0.4μm grain size Grain Cobalt Density Hardness T.R.S Application um % g/cm3 HRA N/mm3 0.4 12 14.05 92.6 4200 High...
|
|
|
|
Stellite 21 ECoCr-E - Cobalt Based Alloy Hard Facing Electrode Medical Applications Hip Implant Product Description WL-Co21 (previously known as WL-Co8) was developed in the mid ...
|
|
|
|
Ultra fine cemented carbide rods endmills blank for glass fiber materials ISO Grade Grain Cobalt Density Hardness T.R.S um % g/cm3 HRA N/mm2 K30-K50 0.4 12 14.05 92.6 4200 ...
|
|
|
|
Stellite 21 Ecocr-E Welding Electrode - Cobalt Based Alloy Hard Facing Electrode Electrical Resistivity Heat Treatments Product Description WL-Co21 (previously known as WL-Co8) was ...
|
|
|
|
OD24.5mm K50 unground carbide rods for high-speed cutting tools ISO Grade Grain Cobalt Density Hardness T.R.S Application um % g/cm3 HRA N/mm2 K30-K50 0.4 12 14.05 92.6 4200 High...
|
|
|
|
Product Description: Hard Facing Rod is a welding rod made of cobalt-based alloy with a stellite 12 green color. It is also known as Bishilite 12 rod. The rod has an international ...
|
|
|
|
High-speed cutting tools with ground carbide rods with chamfer 0.4μm grain size Grain Cobalt Density Hardness T.R.S Application um % g/cm3 HRA N/mm3 0.4 12 14.05 92.6 4200 High...
|
|
|
|
Product Description: Hard Facing Powder Hoganas 2748, also known as Weartech WT-1, is a cobalt-based powder for surface hardening and high wear resistance applications. It is an ...
|
|
|
|
Ultra fine cemented carbide rods endmills blank for glass fiber materials ISO Grade Grain Cobalt Density Hardness T.R.S um % g/cm3 HRA N/mm2 K30-K50 0.4 12 14.05 92.6 4200 ...
|
|
|