Spezilla Tube Co., Ltd. (Shanghai) |
Verified Suppliers
|
|
ASTM B 423 INCOLOY 825 UNS N08825NICEL ALLOY STEEL SEAMLESS TUBING
Incoloy 825 is a nickel-iron-chromium alloy with additions of
molybdenum and copper. This nickel steel alloy’s chemical
composition is designed to provide exceptional resistance to many
corrosive environments. It is similar to alloy 800 but has improved
resistance to aqueous corrosion. It has excellent resistance to
both reducing and oxidizing acids, to stress-corrosion cracking,
and to localized attack such as pitting and crevice corrosion.
Alloy 825 is especially resistant to sulfuric and phosphoric acids.
This nickel steel alloy is used for chemical processing,
pollution-control equipment, oil and gas well piping, nuclear fuel
reprocessing, acid production, and pickling equipment.
What are the characteristics of Incoloy 825?
Alloy 825 (UNS N08825) Chemical Composition,
Ni | Fe | Cr | Mb | Cu | Ti | C | Mn | S | Si | Al |
---|---|---|---|---|---|---|---|---|---|---|
38.0-46.0 | 22.0 min | 19.5-23.5 | 2.5-3.5 | 1.5-3.0 | .6-1.2 | 0.05 max | 1.0 max | 0.03 max | 0.5 max | 0.2 max |
Corrosion Resistance
Alloy 825 has a high level of corrosion resistance. It resists
general corrosion, pitting, crevice corrosion, intergranular
corrosion, and stress-corrosion cracking in both reducing and
oxidizing environments.
In what applications is Incoloy 825 used?
ASTM Specifications
Pipe Smls | Pipe Welded | Tube Smls | Tube Welded | Sheet/Plate | Bar | Forging | Fitting |
---|---|---|---|---|---|---|---|
B423 | B424 | B425 | B564 | B366, B564 |
General Mechanical Properties
Tensile (ksi) | .2% Yield (ksi) |
---|---|
85 | 30-35 |
Alloy 825 has good mechanical properties from cryogenic
temperatures to moderately high temperatures. However, exposure to
temperatures above 1000° F can result in microstructural changes
that significantly lower ductility and impact strength. Alloy 825
should not be used at temperatures where creep-rupture properties
are design factors.
Element | Min | Max |
Nickel + Cobalt | 38.0 | 46.0 |
Cobalt | --- | 2.00 |
Chromium | 19.5 | 23.5 |
Copper | 1.50 | 3.00 |
Iron | 22.0 | --- |
Silicon | -- | 0.50 |
Manganese | -- | 1.00 |
Carbon | -- | 0.05 |
Aluminum | --- | 0.20 |
Form | Standard |
---|---|
Metal Type | UNS N06625 |
Bar | ASTM B446 AMS 5666 BS3076 |
Wire | AMS 5837 |
Sheet | ASTM B443 AMS 5599 BS3072 |
Plate | ASTM B443 AMS 5599 BS3072 |
Pipe | ASTMB444 ASTM B704 AMS 5581 BS3074 GEB50TF133 |
Tube | ASTM B444 ASTM B704 AMS 5581 BS3074 GEB50TF133 |
Fitting | ASTM B366 Din 17754 |
Forging |
|
Weld Wire | |
Weld Electrode | |
NA 21 | All forms |
Din | 2.4856 |