Home Companies Mianyang Baoheng New Material Technology Co.,Ltd

14-4PH Alloy Round Bar 14-4PH Superalloy

Mianyang Baoheng New Material Technology Co.,Ltd
Active Member

Contact Us

[China] country

Address: Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China

Contact name:Bruce Chiu

Inquir Now

Mianyang Baoheng New Material Technology Co.,Ltd

14-4PH Alloy Round Bar 14-4PH Superalloy

Country/Region china
City & Province mianyang
Categories Nickel
InquireNow

Product Details

14-4PH Alloy Round Bar 14-4PH Superalloy
 
 
Description


14-4PH Alloy Round Bar 14-4PH Superalloy is High temperature alloys and other special alloys

All of 14-4PH Alloy Round Bar 14-4PH Superalloy conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

  • Material:Metal, Alloy Round Bar14-4PH
  • Shape:Alloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm
  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm
  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

 
Products Details

 

14-4PH Alloy Round Bar 14-4PH Superalloy

Chemical Composition (weight%):Mechanical Properties Under Final Heat Treatment:
C(%): 0.03
Si(%): 0.75
Mn(%): 0.35
Cr(%): 14.1
Ni(%): 4.25
Mo(%): 2.38
Co(%): —
W(%): —
Al(%): —
Cu(%): 3.25
Ti(%): —
Other(%): Nb 0.25,N 0.02
TS, σb/≥MPa: 268
YS, σ0.2≥/MPa: 782
EL, δ 5≥(%): 13
Impact, AKV≥/J: 11
 

 


Applications:


14-4PH Alloy Round Bar 14-4PH Superalloy is often used in the Aerospace, cylinders, gears, hollow shafts, landing gears, marine gas turbine, etc.

 

 

 


FAQ
 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of raw materials and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

Hot Products

UNS S15500 Stainless Steel Round Bar Description UNS S15500 Stainless Steel Round Bar is a ...
ASTM Grade 410 Stainless Steel Round Bar AISI 410 UNS S41000 Description Our company provides ASTM ...
XM-29 Austenitic STainless Steel UNS S24000 Stainless Steel Round Bar Description XM-29 UNS S24000 ...
303Se Stainless Steel Round Bar UNS S30323 Round Bar Description 303Se Stainless Steel Round Bar UNS ...
W-Nr 1.4571 X6CrNiMoTi 17-12-2 Stainless Steel Round Bar 320S31 Z6CNDT 17-12 Alloy Steel Bar ...
X20CrMo13 W-Nr 1.4120 Stainless Steel Round Bar G-X20CrMo13 Hot Rolled Strips Size Range Round bar / ...