Home Companies Baoji Lihua Nonferrous Metals Co., Ltd.

Gr1 Gr2 Gr5 Titanium Wire Coil

Baoji Lihua Nonferrous Metals Co., Ltd.

Contact Us

[China] country

Trade Verify

Address: Room 2508, 25 / f, Unit 1, Block B, Wanrun International Plaza, Gaoxin 4th Road, Baoji City, Shaanxi Province, China

Contact name:Myrna

Inquir Now

Baoji Lihua Nonferrous Metals Co., Ltd.

Verified Suppliers
  • Trust
    Seal
  • Verified
    Supplier
  • Credit
    Check
  • Capability
    Assessment

Gr1 Gr2 Gr5 Titanium Wire Coil

Country/Region china
City & Province baoji Shaanxi
Categories Titanium Wire
InquireNow

Product Details

Astm b863 gr1 gr2 gr5 gr7 gr12 2.4mm 3.2mm titanium welding wire in coil

 

Titanium welding wire has excellent welding process performance, beautiful weld formation, and its welded metals

have excellent comprehensive mechanical properties.
Mainly used for welding of titanium-based alloys.
Radiographic inspection requirements for weld metal inspection: Grade Ⅰ

 

Product nameTitanium welding wire
StandardAstm b863
Material

Pure Titanium :Gr1. GR2, GR3, GR4

Alloy Titanium :GR5, GR7 ,GR12

Diameter

Spool wire:φ 0.5mm, 0.6mm, 0.8mm (with wire reel)

Coil wire:   φ 1.0, 1.2, 1.6, 2.0, 2.4, 3.0, 4.0, 5.0mm (no wire reel)

Straight wire: φ 1.2, 1.6, 2.0, 2.4, 3.0, 4.0, 5.0, 6.0mm (plastic box packing, 1000mm in length)

Length

Spool wire and coil wire :according to weight

Straight wire:1000mm, or as customer's request

Product situationCold rolled(Y)~Hot rolled(R)~Annealed (M)~Solid Status

 

Titanium wire specifications

A. Titanium wire specifications: φ0.8-φ6.0mm

B. Spectacle titanium wire specification: φ1.0-φ6.0mm special titanium wire

C. Titanium wire specification: φ0.2-φ8.0mm special for hanging tool

 

Grade

TA0, TA1, TA2, TA3, TA4, TA5, TA6, TA7, TA9, TA10, TC1, TC2, TC3, TC4, TC6, TC11, GR1, GR2, GR3, GR5 Ti6AL4V ELI, Ti6AL7Nb, Ti13Nb13Zr, Ti1533

 

standard
GB / T, GJB, AWS, ASTM, AMS, JIS


status
Annealed state (M) Hot-worked state (R) Cold-worked state (Y) (annealed, ultrasonic flaw detection)

surface
Pickled surface bright surface

use
Military, medical, sporting goods, glasses, earrings, headwear, electroplating hangers, welding wire and other industries.

 

 

 

Precautions for using titanium welding wire:

(1) Construction workers and welders should wear clean white gauze gloves (no cotton gloves are allowed).

(2) It is strictly forbidden to touch and touch iron objects by hand in the treated welding area.

(3) Welding work should be performed indoors as much as possible, and the ambient wind speed should be ≤0.5m / s

to avoid being affected by the wind.

(4) When welding, short arc welding should be used as much as possible, with a small welding heat input, and the

angle between the nozzle and the weldment should be 70-80 degrees.

(5) When the butt pipe is positioned and welded, its butt gap is generally about 0.5mm.

(6) Each welding seam should be completed as much as possible. The welding seams must be connected. Before

welding,

the joints should be cleaned. The length of the welding meat overlap is 10-15mm.

(7) When welding, the welding torch should not swing left and right, and the melting end of the welding wire must

not move

out of the gas protection area.

(8) Gas should be supplied in advance when welding arc initiation. Welding torch cannot be lifted immediately when

arc is extinguished. Gas supply should be delayed until the temperature drops below 250 ℃.

(9) The distance between the gas shield and the welding torch should be short, and the gap in contact with the pipe

wall should be small. When performing butt welding of pipes, in order to meet the requirements of single-sided welding

and double-sided forming, the welding is performed in two times: one for back-sealing welding (without filler materials

when back-sealing), and the other for forming welding. In multi-layer welding, the previous bead must be completely

cooled before the next bead is welded.

(10) Welding must be completely cleaned of surface impurities such as oil, rust, and moisture.
(11) To prevent the surface temperature of the bead from excessive oxidation during welding, a tail cover must be

added to enhance the protection effect.

 

Production Process of titanium wire:

Titanium sponge→compacting electrodes→melting→forging→bar billets→hot rolling→cold draw→titanium wires

 

Surface quality: high precision, good finish, no oxidation color, no cracks, peeling, thorns, marks and inclusions. Minor

local scratches, abrasions, spots and pits that do not exceed the allowable deviation of the wire diameter are allowed.

 

 

Detailed pictures:

 

Chemical composition
GradeEssential component<=Impurities <= 
TiAlMnVCONHFe
ERTi-1Remainder0.030.03-0.100.0120.0050.08
ERTi-2Remainder0.030.08-0.160.0150.0080.12
ERTi-3Remainder0.030.13-0.200.020.0080.16
ERTi-4Remainder0.030.18-0.320.0250.0080.25
ERTi-5Remainder5.5-6.753.5-4.50.050.12-0.200.030.0150.22
ERTi-23Remainder5.5-6.53.5-4.50.030.03-0.110.0120.0050.20

 

 

 

Welcome to contact!

Email: fred@lihua-group.com

Phone number (WhatsApp and Wechat): +86 18909172760

 

 

 

Hot Products

GR2 Titanium Stub Ends price ASME B16.9 1. Our Company As a leading manufacturer of titanium ...
CNC machined UNS R50400 UNS R56400 F2 Titanium Flange bl Blind flange BL flange is also know as ...
ASME 16.5 B381 Ti Gr. 2 titanium weld neck flange rf class150 WN forged flange Welding Neck Flanges ...
ASTM B381 titanium Gr F2 Welding Neck Flange Titanium Gr2 Raised Face Flange BLRF Titanium Grade 2 ...
ASME Titanium Flanges Titanium Flange is a part connecting shaft and shaft and is used for ...
The EN 1092-1 Equivalent ASME is one of most common flanging used in the world. The EN 1092-1 Flange ...