Equipment Overview
The determination of vulcanized rubber machine applies a constant strain compression deformation of the test method. This test is compressed to the provisions of vulcanized rubber specimens under a high, after a certain temperature and time, or media infiltration, the determination of the rate of the sample compression set.
Test Fixture:
1. Compression required smooth surface, its finish is not less than
7
2. Compression plateu deformation in the test should not be
proposing to adopt a steel plate, measuring about 75mm, width 50mm,
thickness is 10mm.
3. Limiter height of 8 ± 0.02mm, 7 ± 0.02mm, 6 ± 0.02mm.
4. Incubator should have a continuous blast device, box test
temperature uniformity. Temperature test area inside the
temperature fluctuation range: 100 ℃ The following is ± 1
Centigarde, 100 ~ 200 Centigrade to ± 2 Centigarde.
Technical parameter:
Model | HZ-7010 |
Rubber specimen | Ф28.68(D)12.7mm |
Foam plastic | 50*50*25mm |
Septum thickness | 7.62mm,8.89mm,9.52mm,10.16mm |
Dimension | 20*12*10cm |
Weight | 10kg |