Chongqing Aorun Industrial Co., Ltd. |
|
Quick Detail:
Name | Epoxy Resin 1179 | Application | Apartment, supermarket,hotel,hospital,home |
Mixing Ratio | A: B = 3:1 (By weight) | Curing time | 25C*8-12H or 60C*3H |
Description:
Our Aorun-1179 UV Stabilized Crystal High Table System Bars Wood
materials are finished; By looking at packaging; Ultra Clear epoxy
system for craft epoxy resin is high performance epoxy resin.
Sunlight and other Ultra Violet light sources provide a subtle,
anti-white effect. Applications requiring a hard coating.
1 to 1 can easily be used in terms of pitch; It waters the layers
It keeps its strength in sharp corners; It has excellent air
release quality and a relatively fast epoxy coating setting time,
allowing for a cool heat run up to 160 °F.
Features:
Aorun epoxi curing hardener and Taiwan South Asia resin makes it more environmentally friendly and yellowproof for more longer time.Crystal clear, anti-yellowing, high hardness, anti-scratch,toy grade.
Items | Units/conditions | Technical Data |
Viscosity | Shore-D | 80-85 |
Volume resistivity | 25℃/ Ω./ cm | 4.3x1015 |
Surface resistivity | 25℃/ Ω. | 2.6x1014 |
Dielectric strength | 25℃ KV/MM | 25 |
Coefficient of linear expansion | CM/K | <6.1x10-5 |
Glass transition temperature | ℃ | >90 |
Temperature resistant | ℃ | -60~120 |
Notice:
1. Keep the room clean. The unused glue after opening the cover
should cover the cover well.
2. Frequent contact with this product will cause allergies to some
people's skin, so try to wear rubber gloves when operating this
product.
3. If you enter the eye carelessly, please rinse it with plenty of
water. If it is serious, please see a doctor immediately.
4. Common production tools can be cleaned with alcohol or acetone.
5. The curing time of the product can be accelerated by heating.
The highest temperature is not more than 80 C.
FAQ:
Q1. Will the Table Epoxy Resin turn yellow over time?
A: No, because we add HALS, which is UV protection, it won't change
yellow.
Q2. Does this Table Epoxy Resin tend to scratch over time?
A: Our product is Scratch Resistance, Heat Resistance, Electrical
resistance.
Q3. What is the ideal temperature to make mixtures?
A: The optimal temperature is 25 degrees celsius, because our
laboratory temperature is 25 degrees celsius, but a little hotter
or colder is also ok.
Q4. How long can last if it is not mixed?
A: The shelf life is about 12 months, if you keep it well.
Q5. What payment terms do you accept?
A: Payment for TT, LC at sight. If you have good Credit or we
cooperate long time, the OA, DP, CAD also workable.
Q6. Could you accept OEM for Table Epoxy Resin?
A: Yes, we can do the packing according to your demand, the packing
bag and the label all can do your brand.
Q7: What tool or other material do I need for Table Epoxy Resin?
A: You need a weighing machine and a container to hole the resin.
If do river table or Art Crafts you may need some pigments and