Shanghai Tankii Alloy Material Co.,Ltd |
Verified Suppliers
|
|
Thermal bimetal strip is by the different expansion coefficient of
two or more than two layers of metal or metal solid combination,
and along the entire interface varies with temperature and the
thermal function of shape changes in composite materials.One of
high expansion coefficient become active layer, low expansion
coefficient becomes passive.When requirements with high
resistivity, but heat sensitive resistance performance is
essentially the same type of thermal bimetal series, can be added
between the two layers of different thickness of middle layer as a
shunt layer, is to achieve the purpose of control different
resistivity.
The basic characteristic of the thermal bimetal is changing with
temperature and temperature deformation, resulting in a certain
moment.Many devices use this feature to convert heat energy into
mechanical work to achieve automatic control.Thermal bimetal used
for control system and temperature sensor in the measuring
instrument.
Main features: heat sensitive properties and low resistivity.Under
300 ºC bend straight, can avoid produce far strain at high
temperature
shop sign | Truflex NI | |
With brand | ||
Composite layer alloybrand | High expansion layer | Ni |
middle layer | -------- | |
Low expansion layer | Ni36 |
shop sign | Ni | Cr | Fe | Co | Cu | Zn | Mn | Si | C | S | P |
≤ | |||||||||||
Ni36 | 35.0~37.0 | - | allowance | - | - | - | ≤0.6 | ≤0.3 | 0.05 | 0.02 | 0.02 |
Ni | ≤99.3 | - | ≤0.15 | - | ≤0.15 | - | - | ≤0.15 | 0.15 | - | 0.015 |
Than bending K(20~135ºC) | Temperature curvature F/(greenhouse ~ 130 ºC) | resistivity | Linear temperature / ºC | Allows the use of temperature / ºC | Density (g/cm after) | |||
Nominal value | Allowable deviation | Standard values | Allowable deviation | |||||
Level 1 | Level 2 | |||||||
10.0 | ±8% | ±10% | 19.0%±10% | 0.17 | ±10% | -20~180 | -70~400 | 8.4 |
Modulus of elasticity E/GPa | Hardness (HV) | Tensile strength MPa | Allow stress MPa | ||
High expansion layer | Low expansion layer | minimum | biggest | ||
152~181 | 185~235 | 200~255 | 588~686 | 98 | 294 |
production process
Cold rolled →go oil → pickling → annealing cold-rolled →oil →
pickling → annealing cold-rolled → conform to the requirements of
the use of thermal bimetal strip
2.Usage
It is mostly used in small transformers, pulse transformers,
relays, transformer, magnetic amplifier, electromagnetic clutch,the
reactor coreand magnetic shielding which work inweak magnetic
orsecondary magnetic field.
3.Features
1).Low coercivity and magnetic hysteresis loss;
2).High resistivity and loweddy-currentloss;
3).High initialmagnetic permeability and maximum magnetic
permeability;
4).High saturation magnetic flux density;
4. Packing detail
1). Coil (plastic spool) + compressed ply-wooden case + pallet
2). Coil (plastic spool) + carton + pallet
5. Products and services
1). Pass: ISO9001 certification, and SO14001cetification;
2). Fine after-sale services;
3). Small order accepted;
4). Fast delivery;