Anti Oxidant Superalloy Tungsten Carbide Plate For 3D Curved Glass Molding Machine

Zhuzhou Zhenfang Yaguang Tungsten Molybdenum Co., LTD.
Active Member

Contact Us

[China] country

Address: Block. 7, Zone C, Auto Parts industrial Park, Tianyuan Dist., Zhuzhou, Hunan, China (Mainland)

Contact name:Shirley Pan

Inquir Now

Zhuzhou Zhenfang Yaguang Tungsten Molybdenum Co., LTD.

Anti Oxidant Superalloy Tungsten Carbide Plate For 3D Curved Glass Molding Machine

Country/Region china
City & Province zhuzhou hunan
Categories Other Metals & Metal Products
InquireNow

Product Details

 

Anti-oxidant superalloy tungsten carbide plate for 3D curved glass molding machine

 

Tungsten carbide heating plate is used on 3D curved glass molding machine, generally 6pieces for one set. Our carbide plate for 3D glass molding machine have high temperature resistant(over 800℃), high thermal conductivity.

 

Product Description
Product Name
super hard alloy cemented tungsten carbide plate for 3D curved glass bending machine
Material
tungsten carbide+Cobalt+Ni+Al+Cr etc.
Function
application for processing 3D mobile phone and watch glass hot bending molding machine
Package
by wooden case

 

Grade Information

GradeISO RangeCobalt%

Density

g/cm3

Hardness

HRA

YG8K30814.889.5
YG6K20614.9590.5
YG6XK10614.9591.5
YL10.2K301014.591.8
YG15K40151487.5

 

Product application

Application Are: 3D Hot bending Glass Molding Machine

Super hard alloy tungsten carbide plate, mainly application for 3D curved glass hot bending molding machine , is widely used to process and form 3D curved glass of mobile phone, watch and TV. Compared with conventional tungsten steel plate and cemented carbide series, super hard alloy composite carbide plate has higher hardness, better high temperature deformation resistance, higher thermal conductivity and thermal diffusion coefficient when used at 900 ℃ high temperature . More stable performance greatly improves the production efficiency.

 

 

 

  • Product Advantages:

1. Excellent tensile strength:500-600MPa at 900 ℃;
2. High thermal shock resistance:fast heating up and cooling down available;
3. Good processability: workable in any condition according to customers’ need;
4. Super high temperature corrosion resistance: long service life without coating;
5. Strong chemical stability:No chemical reaction with glass,graphite and nitrogen;

6. Energy saving,environmental protection,good appearance of products.

If have any more information, please feel free to contact with me.

 

Web:www.tungstencarbide-rods.com
Tel: 0086-731-28215800
Fax: 0086-731-28215800
Mobile: 0086-13823202651(wechat/whatsapp)

Email address:sharon@chinahardalloy.com

3-200403102031620.png

 

Hot Products

Sintered Blank K10 tungsten carbide tube/pipe for thermocouple sleeve Detailed Product Description 1...
Good Wear Resistance Tungsten Carbide Metal Tube With One End Closed Our tungsten carbide rod blanks ...
Tungsten Carbide Flat Bars 136x19.6x1.6mm For Making Cutting Blade Tungsten carbide strips is a ...
Factory supply ground original tungsten carbide thin wall tube, cemented carbide pipe Applications: ...
Factory supply ground original tungsten carbide thin wall tube, cemented carbide pipe Applications: ...
High Precision Ground Tungsten Carbide Needle/Pin With High Hardness Product Description We offer ...