Home Companies Sun On Plastic Moulding Limited

ISO Shrinkage Injection Moulding Solutions OEM

Sun On Plastic Moulding Limited

Contact Us

[China] country

Trade Verify

Address: Room 101, Building 1, No. 8, Hongying Erheng Road, Fenggang Town, Dongguan City, Guangdong Province

Contact name:Project Manager

Inquir Now

Sun On Plastic Moulding Limited

Verified Suppliers
  • Trust
    Seal
  • Verified
    Supplier
  • Credit
    Check
  • Capability
    Assessment

ISO Shrinkage Injection Moulding Solutions OEM

Country/Region china
City & Province dongguan guangdong
Categories Mechanical Transmission Parts
InquireNow

Product Details

The Cause And Countermeasure Analysis Of Shrinkage In Products

Reprint Books In A Reduced Format

Shrinkage refers to the depression of the product table and the production of insects, like hair in the thicker part of the wall. In the process of cooling the molten resin from the external part, when the volume shrinkage cannot be compensated, the resin on the surface of the formed product is subjected to the volume shrinkage of the molten resin in 6 parts, resulting in the formation of q marks.

 CauseCuntermeasure
Forming condition

1. There are many cases of insufficient pressure and retaining pressure during the injection period

2. The pressure retention time is insufficient

4. The mold temperature is not appropriate, the mold temperature is too low, the gate curing fast, pressure retention failure is easy to produce shrinkage hole: the mold temperature is too high, setting the appropriate mold temperature is easy to produce shrinkage marks

5. The injection speed is too fast

The temperature of the material is too high, and the shrinkage of the material is too large

1. Increase the injection pressure and pressure holding pressure; 2. Increase the pressure raising time

3. Increase the measurement distance

4. In thick products, this tendency is stronger and the speed is reduced

5. Properly reduce the temperature of the material

 

Die

1. The runner and gate are too small. 2. Improper placement of pouring II makes the material flow distance too long

3. Insufficient or inconsistent mold cooling

 

1. Increase the section of runner and gate

2. Review runner and gate

3. Check the cooling system

 

Product Design

1. Uneven thickness

2. The shape of tendons is not standard

 

1. Avoid uneven thickness, can use stolen thick pin or groove.

2. Avoid thick and long tendons

Material

1. The shrinkage rate of materials is too large

2. Poor material fluidity

 

1. Switch to materials with low shrinkage

2. Improve material mobility

OtherScrew check ring is damagedReplace the check ring

 

Hot Products

OEM traffic lights, auto warning lights ABS/PP plastic parts Product details We can offer the full ...
OEM high quality medical arm sleeve front shell-ABS plastic parts Description Mould material 45#, 50...
Daily plastic parts can be customized Description Mould material 45#, 50#, P20, H13, 718, 2738, ...
High Quality Injection Plastic Parts for ABS PP PE PC Plastic Material Product details We can offer ...
Single Or Multi-Cavity Injection Molded Parts With Smooth Surface Finish Product Description: ...