Industry Polyester Dust Collector Filter Bag For Cement Mine Iron Pharmacy Bag House High Precision Filter Bag
Polyester (PE) filter bags
Polyester needle felt is made from polyester fabric by needle punch, and treat with singeing, calendering ,heat-setting process. This material has good friction resistance, high porosity, good twist resistance, good air permeability. It is a kind of wildly applied normal temperature needle felt .
We also provide FMS/ Fiber Glass/ PPS... filter bags, choose the material according to site situation.
Our capacity: 20,000 per month (standard product)
Size: Customization Accepted
Optional process: Sewing or hot welding
Filtration precision: ≤30mg/m³ (laminating PTFE film, ≤5mg/m³)
Finish-treatment: Calendering, Heat setting, Singeing
Optional Choice: Pleated Filter Bag (Star Bag)
The main advantages and features:
1. To increase system filtration capacity by 50-150% as needed without major changes to the dust collectors ;
2. System cleaning efficiency markedly increased with the effective increase of bag to bag distance;
3. Bag life extended due to significant reduction of fatigue damage to the bags due to bag to cage impact.
| | Polyester (PET) with PTFE membrane | | | | |
Weight (g/m2) | 500 | 500 | 750-800 | 500 | 500-550 | 450-600 |
Thickness (mm) | 1.7-2.0 | 1.7-2.0 | 1.2-1.6 | 2.1 | 1.8-2.0 | 1.9-2.4 |
Running Temperature (°C) | 130 | 130 | 240 | 180 | 160 | 200 |
Peak Temperature (°C) | 150 | 150 | 260 | 260 | 190 | 240 |
Air Permeability (M3/M2.S. 200Pa) | 8-12 | 8-12 | 5-8 | 14 | 15 | 8-12 |
Mechanical Finish | Singeing, calendaring, heat-set | Singeing,calendaring | Heat-set and Singed one side | Singeing | Singring coating Heat-set | Singeing |
Chemical Finish | membrane | PTFE/Teflon Water and oil repellent | PTFE impregnated peritoneal | | | PTFE coating, membrane |
Warp Of Stretch Strength | 800 | 1000 | 600 | 900 | 900 | 900 |
Welf Of Stretch Strength | 1200 | 1300 | 800 | 1200 | 1200 | 1200 |
Resistance to Acid | Medial | Fair | Excellent | Excellen | Excellent | Fair |
Resistance to Oxidation | Excellent | Good | Excellent | Excellent | Poor | Fair |
Resistance to Alkali | Medial | Poor | Excellent | Excellent | Excellent | Good |
Resistance to Hydrolysis | Medial | Poor | Excellent | Excellent | Excellent | Fair |
Application | 1) The fume and smoke treatment and particle removing system in metallurgy plant 2) Smoke filtration in garbage burning, coal-feed boiler,power plant 3) Asphalt concrete mixture, cements, chemical,ceramics, building materials 4) Dust treatment, purification and collection in electronics, mining, flour and timber processing |
Size | Φ4'' ; 5'' ; 5.25'' 6'' ; 6.62'' Length: 18'' up to 192'' |
Filter Bag Top Construction | 1) Side Load: raw edge top (3” longer than split collar cage length) 2) Top Load: snap band/ring ; double beaded |
Bottom Construction | 1) Single-ply felted disc bottom 2) 3” bottom; double-ply wearguard 3) 5” wear cuff with 2” overhang below bag disc bottomBottom Construction |
Product Show
Produce process:
1)Fiber:high grade Aramid fiber
2)Scrim: Aramid/PTFE
3)Produce Process:needle punched
4)Filter Felt Weight: 550±20gsm
5)Filter Felt Thickness: 2.0±0.2mm
6)Finish treatment:Singeing, calendaring, PTFE dipping
7)Laboratory Testing:check the test report below
8)Cut according to customer's requirement
9)Packing according to customer's requirement
Precautions for dust bag installation
1. Old cloth bags of the new process should not be mixed, to avoid different damage time and affect the normal operation of the dust removal equipment.
2. Aging of cloth bags. Mainly due to the following reasons, a cause investigation is needed, corresponding measures are taken and the dust filter bag is replaced.
1).Due to abnormal high temperature and hardening shrinkage; 2). Due to contact with the acid, alkali or organic solvent vapor reaction; 3).React with moisture.
3. The filter cloth should not be hung too tightly or too tightly. It is easy to accumulate dust if it is too loose.
4.Replace the cloth bag, blow it with compressed air first, and then check if there are any holes. After the holes are repaired, leave them for replacement. As dust
Rinse the cloth bag, rinse it with water, and leave it for replacement after drying.
5.Blockage of dust bag. When the bag is clogged, the resistance increases, which can be expressed by the reading of the differential pressure gauge. Cloth Closure
plugs are the main cause of wear, perforation, and shedding of bags. The cause of the clogging of the dust bag is checked and repaired as follows.
1).Temporarily strengthen the dust removal to solve the clogging of the bag; 2).Replace the bag partially or completely; 3).Adjust the installation and operating conditions.
FAQ
Q1. How about your delivery time? |
A1: Generally, it will take 7-30 days after receiving your advance payment. The specific delivery time depends on the items , transportation ways and the quantity of your order.
Q2. Can you produce according to the samples? |
A2: Yes, we can produce by your samples or technical drawings. We can build the molds and fixtures.
Q3. Is it convenient to install and operate the equipment? |
A3: Convenient, we will take a one-to-one service for customers, for each customer tailored for your product equipment and a complete set of solutions.
Q4. What is your terms of payment? |
A4: T/T 30% as deposit, and 70% before delivery. We'll show you the photos of the products and packages before you pay the balance.
Q5. Can it really meet the environmental requirements? |
A5: Ensure that customers meet the environmental standards, the environmental situation of the current 10 mg high emission standards.
Q6. What if the equipment is broken? |
A6: If any problem occurs during the warranty period, we will try our best to solve it and achieve customer satisfaction.After the warranty period of equipment supporting wearing parts to provide 10% discount policy, and to ensure that customers in the use of no worries.